On-Demand Course: Chloride Limits and Thresholds for Concrete: Perspectives in Laboratory Testing and Modeling Techniques

Price: $ 39.00 USD

Choose Product Language

Choose Product Units


Choose Product Format

Quantity:


Notes/Preview

The contents of this course include three recorded presentations from the ACI 2015 Fall Convention:

• Threshold Values in Concrete—A Look Back and Ahead by Ueli M. Angst, Swiss Federal Institute of Technology

• Confusion on Chloride Limits in Specifications that Challenge the Industry by Colin L. Lobo, National Ready Mixed Concrete Association

• Examining Factors that Influence Service Life Model Predictions by W. Jason Weiss, Oregon State University

INSTRUCTIONS: Study the materials included in this module. Then, complete and pass the corresponding 10-question quiz with a score of 80% or higher to receive a certificate for 0.1 CEU (equivalent to 1.0 PDH). This online course is not approved for credit with the Florida Construction Industry Licensing Board (CILB).

Continuing Education Credit: 0.1 CEU (1 PDH)

Approved by AIA and ICC

Access Period: 30 days

Description

Field studies, laboratory testing, and modeling of chloride concentration limits and threshold levels that initiate reinforcement corrosion vary in their predictive abilities. Corrosion initiation measurements for portland and blended cement concretes can lead to better service life predictions. However, chloride limits vary across industry guides and specifications. This course covers material sources of chlorides and clarifies ACI’s allowed chloride limits for concrete used in different types of structures. The effects of calcium chloride diffusion and chloride binding at reinforcing bars on time to corrosion are also explored.

 

Document Details

Publication Year: 2017

ISBN:

Categories: Corrosion

Formats: Online Learning

Table of Contents

Learning objectives:

1. Describe variances in chloride limits used by ACI and other international standards organizations.

2. Identify factors known to influence chloride thresholds in concrete.

3. Apply current research on chloride thresholds and effects of chloride concentration versus temperature for concrete containing supplementary cementitious materials (SCMs).

4. Describe the effects of differing concentrations of soluble calcium chlorides with Type I cement concrete and temperature changes.

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Quantity Discounts

This item qualifies for quantity discounts. Discounts are reflected in the shopping cart.
Quantity Discount
10 - 19 25%
20 - 49 35%
50+ copies 50%